NSF Series Water Reducer Agent

View More

  • NSF Series Water Reducer Agent
  • NSF Series Water Reducer Agent

NSF Series Water Reducer Agent

  • MOQ: 1000 kg
  • Supply Capability: 500000 kg / month
  • Port: Qingdao
  • Delivery: prompt
  • Packaging: 25kgs / 50kgs / 750kgs net per bag.

Details

WATER REDUCER FDN-A  

(1) . PROPERTIES,FEATURES&CHARACTERISTICS (FDN-A)  

 1. Appearance: Light brown powder & dark brown liquid, Non-poisonous, odorless, non-flammable and non-corrosive to steel bars.  

 2. Remarkable Plasticity: As a condition of blending where amount of cement and collapsibility are fixed aforehand, mixing water can be decreased by 18-28% when it is admixed with reinforced concrete at 0.5-1.0%. Statistically, compression strength on the 1 st  day,  the 3 rd  day and the 28 th  day after single application is increased by 60-90% and 25-60% respectively when it is added at standard blend dosage. As the result, compression strength,  tensile strength, buckling strength and modulus of elasticity will be improved to some extent.  

3. Improve miscibility of concrete amalgamator with water and collapsibility as well. As a condition of equivalent blending, collaposibility can be increased 5-8 times when it is added at 0.75% blend dosage.  

4. 15-20% of cement can be reserved when the agent is blended at 0.75% blend dosage, which is preconditioned  by same collapsibility and strength.  

(2) . PARAMETERS&ACCEPRANCE CRITERIA (FDN-A) 

ITEM  

FDN-A  

ITEM   

FDN-A  

Solids content (%) 

≥92%  

PH value  

7-9  

Na2SO4 content(%)  

﹤  5%  

Net starch fluidity (mm)  

≥250mm 

Content of Chloride (%)  

﹤  0.3% 

Surface tension (N/m)  

(70 ± 1) *10 -3  N/m 

(3) Parameters &acceptance criteria (FDN-A for reference ) 

Parameters  

Criteria 

Actual results  

Parameters   

criteria  

Actual results  

Water reduction  %  

≥14  

18-28  

Compression  

Strength,% 

1d  

≥140  

170  

Water penetration  %  

≤90  

79  

3d  

≥130  

160  

Air content   %  

≤3.0  

1.6  

7d  

≥125  

145  

Temporal distribution   

for setting    

(min) 

Initial   

setting time  

-90~+ 120  

-90  

~+120  

28d  

≥120  

135  

Terminal   

setting time 

Shrinkage, %  

28d  

≤135  

82  

Corrosion to steel bars  

None 

None   

Nate: standard blend dosage: 0.75% (as cement amount)  

(4) USAGE:  

 1. Blending dosage at 0.5%-1.0%,0.75% mixing dosage advised.  

 2. Prepare solutions as required.  

 3.Direct use of powder agents is allowed. Alternatively the addition of the agents is followed by water  moisturization (water-cement ratio:60%).  

 4. The agent can be combined with other extemally applied agents if pilot development or laboratory experiment succeeds.  

You may also be interested in the following product(s)